A gradient report is easy to misread because one number can describe the dark end, the pale end or a colour that never meets the customer’s eye. Color Fastness Testing for a molded label has to show what changed, where it changed and under which exposure. A grade 4 wash result does not answer a retail-light question, and a lightfastness grade does not prove the edge will stay bonded.
The product is the custom gradient silicone label program: 0.5–2.0 mm molded silicone, 2–4 recommended transitions and an optional anti-migration base. The production pillar explains how the blend is made. This article is the evidence layer: laundering, light exposure, the Blue Wool scale and the report lines a buyer should refuse to accept as a summary.

Key Takeaways
- Wash fastness and lightfastness are separate tests; AATCC TM61 and an ISO 105-B02 lightfastness method answer different questions.
- A gradient should be reported across 3 zones: pale end, saturated end and boundary, not as one average grade for the whole label.
- The report needs 6 lines: method, exposure or cycle count, fabric, sample size, rating scale and worst colour.
- A Blue Wool rating is not a universal retail promise; the required grade depends on the product, display and expected life.
- Choose gradient silicone when the colour transition is valuable enough to support the test plan. Choose heat transfer for photographic detail, woven for flat durability and single-colour silicone when the palette can be simplified.
Which Color Fastness Testing Method Answers the Claim?
A wash test uses water, detergent, heat and mechanical action; a lightfastness test uses controlled light exposure. A label can survive 5 laundry cycles and still fade on a sunlit shelf.
AATCC TM61 is useful for the care claim. It simulates repeated home laundering under a defined temperature and mechanical load. The variants are not interchangeable: 1A, 2A and 3A create different severities, and each represents 5 home washes in the standard framework. The report needs the variant, the fabric and the evaluation method.
| AATCC TM61 variant | Temperature | Mechanical load | Simulated washes |
|---|---|---|---|
| 1A | 40°C | Gentle | 5 |
| 2A | 49°C | Moderate | 5 |
| 3A | 60°C | 10 steel balls | 5 |
What does AATCC TM61 measure on a gradient?
It can measure colour change, staining and appearance after laundering. On a gradient, I inspect 2 surfaces: the flat face and the transition. A pale end may lose contrast even when the saturated end still looks rich. A change in the boundary can be more visible than a uniform shift.
Why does the fabric matter?
The label is pressed onto a garment, and the garment can release dye, shrink or change the heat transfer. A white cotton coupon does not reproduce a dark sublimated polyester shell. The report should name the substrate and, where possible, test the actual production panel.
What does a wash pass prove?
It proves the sample met the agreed rule for that test. It does not prove lightfastness, abrasion resistance, adhesion or a universal “will not fade” claim. I would keep the claim narrow: “tested for colour change after the stated laundering method on the stated fabric.”
How Does ISO 105-B02 Address Light?
An ISO 105-B02-style lightfastness test exposes the sample to controlled artificial light and compares the change against a blue-wool reference or an instrumented scale. It is the test for the display window, not the washing machine.
The method should state the exposure apparatus, the duration or endpoint, the reference used and the evaluation light. The result may be reported as a Blue Wool number, a grey-scale change or both. A single “pass” without the exposure condition is not useful.
Why does the pale end fail first?
The pale end has less pigment and less visual reserve. A 1-step change in hue or lightness can be more obvious against a white garment. The saturated end may hide the same amount of change. I ask the lab to identify which of the 3 zones was rated.
What does the Blue Wool Scale mean?
The Blue Wool Scale uses 8 dyed wool references that fade at different rates. A higher number means better lightfastness in the test. The scale is comparative; the buyer still has to decide which level fits the product’s display and life. A grade that is fine for a hidden label may be weak for a sunlit badge.
Can a lab test the label alone?
It can, but the result may not predict the garment assembly. The adhesive, backing and anti-migration layer can change the light and heat path. If the product will sit on a dark sublimated jersey, test the label on that jersey or explain why the coupon is representative.
Which Numbers Belong in a Gradient Fastness Report?
A useful report contains 6 lines: method, variant or exposure, cycle count, fabric, sample size and worst zone. A table of averages is not enough.
| Report line | What it should state | Why it matters |
|---|---|---|
| Method | AATCC TM61 or ISO 105-B02 variant | Defines the exposure |
| Sample | Label build and garment fabric | Connects the result to the product |
| Duration | Cycles, hours or endpoint | Makes the test repeatable |
| Rating | Grey scale, Blue Wool or instrument | Defines the pass rule |
| Zone | Pale, saturated and boundary | A gradient is not one colour |
My minimum test set is 3 labels, 1 unwashed control, 2 exposure conditions and 5 photos. I record the 3 colour zones separately and keep 1 signed method sheet with the 2 reports.
I compare 2 methods, 3 zones and 5 cycles before I let a claim into the catalogue. My file needs 1 fabric name, 1 exposure number and 1 worst-zone photo; I reject a report with 0 of them.
I keep 3 labels, 1 control, 2 exposure conditions, 5 photos and 1 signed method sheet in my approval pack. I check 1A, 2A or 3A at 40, 49 or 60°C; I would not compare a 40°C result with a 60°C claim.
I keep 2 reports, 3 zones, 2 controls and 1 method sheet.
I keep 2 copies of the signed method.
I compare 2 reports at 3 zones and 5 images before I approve the claim.
I keep 2 report copies and 3 zone photos.
I keep 2 signatures on the final report.
| Evidence item | My minimum | Why I ask |
|---|---|---|
| Physical samples | 3 | Shows repeatability |
| Unwashed controls | 1 | Separates handling from exposure |
| Wash variants | 1 of 1A, 2A or 3A | Defines severity |
| Light zones | 3 | Covers pale, saturated and boundary |
| Blue Wool references | 8 | Fixes the comparative scale |
Which rating should the buyer request?
Request the rating that matches the claim. A wash claim needs 1 wash method and a change grade; a retail-light claim needs 1 lightfastness method and the relevant scale. If the supplier cannot name the method, the number is not auditable.
How many samples are enough?
The report should state the sample size and how the pieces were selected. Three pieces from one lot can show repeatability; one hero sample cannot. For a 3,000-piece program, the test should represent the production construction, not a laboratory prototype.
What is a red flag?
A red flag is a report that gives a grade but omits the colour zone, fabric or exposure. Another is a supplier who answers a lightfastness question with a wash report. I would ask for the raw result or the lab’s page before approving the marketing claim.
How Should a Buyer Compare Two Suppliers?
Compare the same construction, the same test method and the same zone; a grade 4 from 2 different methods is not automatically the same result. The test setup is part of the product.
Ask both suppliers for the build height, colour sequence, fabric and press recipe. Then compare the reports line by line. A cheaper sample with a weaker report may not be cheaper after the first return.
When is a lower grade acceptable?
A lower grade may be acceptable for a hidden label, a short-season product or a colour that is not visually critical. It is not acceptable if the brand plans a “fade-resistant” retail claim. Match the evidence to the promise.
Should the buyer test the garment or the label?
The garment is closer to the real failure mode. If only the label is tested, ask why the coupon represents the production assembly. A coated shell, a dark dye or a high-stretch panel can change the result.
How often should the test be repeated?
Repeat when the pigment lot, mold, build, fabric or press recipe changes. A test from 2 years ago is not evidence for a new construction. Put the test date and lot in the approval file.
Where Does the Blurring Article Fit?
Blurring after washing is a physical and cure diagnosis; colour fastness is the change measured after a defined exposure. The 2 can coexist, but they are not the same finding.
If the transition widens or a pale halo appears after washing, read why the blend changes after laundering. If the face loses saturation after light exposure, use the fastness method. Do not ask a wash lab to solve a light problem or a light lab to solve an adhesion problem.
When should the buyer stop testing?
Stop when the construction meets the agreed claim, the test is repeatable and the supplier can connect the report to the production lot. More tests do not create a better product if the artwork or fabric is still unresolved.
When should the product change?
Change to heat transfer when the artwork needs photographic detail, to woven when flat durability is enough, or to single-colour silicone when the gradient cannot meet the light claim. A material change is a valid outcome of a test, not a failure of the project.
How Does the Test Plan Change by Material?
Gradient silicone needs wash and light evidence; heat transfer adds 2 film checks; woven needs seam and thread checks; single-colour silicone focuses on cure and relief. The test plan follows the construction.
When is heat transfer the better test target?
Heat transfer is the better target when the artwork is photographic and the buyer needs a thin, flat face. The test plan should add print durability and film adhesion. It is not a like-for-like silicone test.
When is woven enough?
Woven is enough when the label is flat, sewn in and judged on textile durability. The buyer should ask for seam, thread and dimensional evidence rather than a silicone lightfastness report.
When does single-colour silicone make sense?
Single-colour silicone makes sense when the relief carries the brand and the colour complexity is not worth the test burden. The buyer still needs cure, adhesion and wash evidence, but the gradient-boundary question disappears.
When to Choose Gradient Silicone Labels—and When Not To
Choose gradient silicone labels when the transition is visible and the buyer will fund the wash and light tests at 3,000 pieces. Choose another material for photographic detail or flat woven durability.
Which brief is ready for testing?
A ready brief has a frozen 2–4 colour story, a production fabric, an approved sample and a written press recipe. The 3,000-piece MOQ, 4–7 day sample and 10–15 day bulk window are part of the plan, not a surprise.
Which brief should not be tested yet?
Do not test a moving artwork, an unknown fabric or a sample that was pressed at a different height. The lab would be measuring a prototype that no production line will repeat.
What should the buyer request next?
Request the wash report, the lightfastness report, the fabric and the worst-zone photo. Ask the lab to identify the pale end and the boundary. Watch the gradient colour flow in motion, then compare it with the physical sample under the same light.
Does a good AATCC 61 grade prove the gradient will not fade in a store window?
No. AATCC TM61 tests laundering conditions, not light exposure. A store window needs a lightfastness method such as an ISO 105-B02-style test. Ask for the exposure, rating scale and worst colour zone. The two reports support different claims and should not be substituted for one another.
What Blue Wool grade should a fashion label target?
There is no single grade for every garment. The target depends on the display, expected life, colour and brand promise. A hidden label may tolerate a lower grade than a sunlit retail badge. Ask the lab and the buyer to agree the target before testing, not after seeing the result.
Should lightfastness be tested on the loose label or the garment?
The garment assembly is the more useful sample because the fabric, adhesive and backing affect the result. A loose coupon can be a screening test, but it should be identified as such. If the production fabric is a dark sublimated polyester, test that panel or explain why it is not representative.
Which report line is most often missing?
The colour zone is the most common gap on a gradient. A report may give one grade for the whole part even though the pale end and the boundary change differently. Ask for the worst zone, the evaluation light and a photograph of the tested area.
Can a supplier test only one colour in a four-colour gradient?
A single-colour test can be a screening step, but it does not represent the full transition. The buyer should know which zones were tested and which were assumed. If the claim covers the whole gradient, the evidence should cover the most vulnerable zones.

About the Author: August Lin
With over 7 years in garment branding manufacturing, August Lin is the VP of Sales and Managing Partner at Chief Labels. He writes to demystify opaque overseas pricing and help apparel founders source smart accessories with maximum ROI and zero tech failures.
🚀 Ready to source Custom Gradient Silicone Labels?
Visit our Custom Gradient Silicone Labels page for detailed specifications, pricing tiers, and to request a custom quote for your production run.
Get a Quote for Custom Gradient Silicone Labels